Dear sir,
we have the waffle slab having the required concrete strength 38Mpa and the columns and the shear wall 50Mpa
we have crushed the concrete cylinders of slab after 28 and 56days but we could'nt reached the required strength as per ACI code .
then we have taken the concrete core sample from different location 3 sample from main beam and 3 from ribs beam and all are failed atleast a single sample not reached to 75% of design strength as 38Mpa we got maximum value out of 6 sample 24Mpa. again taken 4 sample from different location all are main beams , all cores are failed ,single sample not reached to required strength as 75% of design strength got maximum value 23.73Mpa.
In such scenario can you suggest us what should we go to strengthen the concrete slab......is there any solution or we have go for demolished the slab (area of slab 1214.45Sqm )
we have the waffle slab having the required concrete strength 38Mpa and the columns and the shear wall 50Mpa
we have crushed the concrete cylinders of slab after 28 and 56days but we could'nt reached the required strength as per ACI code .
then we have taken the concrete core sample from different location 3 sample from main beam and 3 from ribs beam and all are failed atleast a single sample not reached to 75% of design strength as 38Mpa we got maximum value out of 6 sample 24Mpa. again taken 4 sample from different location all are main beams , all cores are failed ,single sample not reached to required strength as 75% of design strength got maximum value 23.73Mpa.
In such scenario can you suggest us what should we go to strengthen the concrete slab......is there any solution or we have go for demolished the slab (area of slab 1214.45Sqm )