Robbiee
Structural
- Jan 10, 2008
- 285
The contractor missed a corbel that supports a precast spandrel beam at one level and at another level they provided rebars not per drawings. The attached sketch provides more info. What would you do to fix these two problems? The architect did not accept a steel bracket. It has to be concrete. Thanks for the help.