Dears, i need your support in judging on the concrete compression test results.
the test have been done after 7days & 28days, on cylindrical shape (300x150mm) and the design strength is C30 and the cement (kg/cu.m) = 360, the results as below:
7 Days age:
Sample (1-A) = 24.3 MPa
Sample (1-B) = 24.6 MPa
Sample (1-C) = 25.5 MPa
Sample (2-A) = 26.5 MPa
Sample (2-B) = 27.7 MPa
Sample (2-C) = 24.3 MPa
Sample (3-A) = 27.0 MPa
Sample (3-B) = 24.7 MPa
Sample (3-C) = 25.5 MPa
28 Days age:
Sample (1-D) = 24.88 MPa
Sample (1-E) = 24.87 MPa
Sample (1-F) = 27.56 MPa
Sample (2-D) = 24.84 MPa
Sample (2-E) = 23.55 MPa
Sample (2-F) = 27.52 MPa
Sample (3-D) = 24.0 MPa
Sample (3-E) = 23.16 MPa
Sample (3-F) = 28.78 MPa
According to the above results, it means that this concrete is failed?
Thanks in advance
the test have been done after 7days & 28days, on cylindrical shape (300x150mm) and the design strength is C30 and the cement (kg/cu.m) = 360, the results as below:
7 Days age:
Sample (1-A) = 24.3 MPa
Sample (1-B) = 24.6 MPa
Sample (1-C) = 25.5 MPa
Sample (2-A) = 26.5 MPa
Sample (2-B) = 27.7 MPa
Sample (2-C) = 24.3 MPa
Sample (3-A) = 27.0 MPa
Sample (3-B) = 24.7 MPa
Sample (3-C) = 25.5 MPa
28 Days age:
Sample (1-D) = 24.88 MPa
Sample (1-E) = 24.87 MPa
Sample (1-F) = 27.56 MPa
Sample (2-D) = 24.84 MPa
Sample (2-E) = 23.55 MPa
Sample (2-F) = 27.52 MPa
Sample (3-D) = 24.0 MPa
Sample (3-E) = 23.16 MPa
Sample (3-F) = 28.78 MPa
According to the above results, it means that this concrete is failed?
Thanks in advance