DtaylorStructeng
Structural
Investigating the moment capacity of some 1200 reinforced concrete Piles.
Due to a bad pour the cover has been compromised and has reduced strength, say 40Mpa in for 50Mpa design strength.
There are inclusions and voids in the cover region of the piles due to issues with bentonite. Some reo was exposed when investigated. The internal diameter within the bars appears sound after investigation.
The problem: There will be a reduced section capacity, I am going to do an analysis with Moment interaction diagram neglecting any cover, (ag cover = 0) for the structural analysis.
However with the cover compromised, can you still develop stress in the steel without the full bond of the bars within the concrete matrix?
Any ideas?
Due to a bad pour the cover has been compromised and has reduced strength, say 40Mpa in for 50Mpa design strength.
There are inclusions and voids in the cover region of the piles due to issues with bentonite. Some reo was exposed when investigated. The internal diameter within the bars appears sound after investigation.
The problem: There will be a reduced section capacity, I am going to do an analysis with Moment interaction diagram neglecting any cover, (ag cover = 0) for the structural analysis.
However with the cover compromised, can you still develop stress in the steel without the full bond of the bars within the concrete matrix?
Any ideas?