concreteworld
Civil/Environmental
Hi,
Please advise what standards/codes we can refer to close a low compressive strength case where in a set of 6 cylinder samples taken from one composite sample, 1 result is fail and the other 5 are okay. The concrete grade is 45 Mpa.
Results are as below
56.1 Mpa
46.4 Mpa
40.3 Mpa
53.5 Mpa
55.9 Mpa
45.8 Mpa
Appreciate your responses...
Thanks in advance
Please advise what standards/codes we can refer to close a low compressive strength case where in a set of 6 cylinder samples taken from one composite sample, 1 result is fail and the other 5 are okay. The concrete grade is 45 Mpa.
Results are as below
56.1 Mpa
46.4 Mpa
40.3 Mpa
53.5 Mpa
55.9 Mpa
45.8 Mpa
Appreciate your responses...