Hi,
Please advise what standards/codes we can refer to close a low compressive strength case where in a set of 6 cylinder samples taken from one composite sample, 1 result is fail and the other 5 are okay. The concrete grade is 45 Mpa.
Results are as below
56.1 Mpa
46.4 Mpa
40.3 Mpa
53.5 Mpa
55.9 Mpa
45.8 Mpa

Appreciate your responses...
Thanks in advance
 
Replies continue below

Recommended for you

Where are you located and what is the governing code for your construction?
 