Compression set data

Status
Not open for further replies.

LeeEccles

Mechanical
Sep 30, 2004
8
Does anyone have any data regarding compression set values for Melinex 378 and Kapton 100 HN films? (i.e. the percentage permanent deformation that occurs under a sustained load).

I know, its a long shot ...
 
Replies continue below

Recommended for you

Melinex is bi axially oriented PET. There might be some data available from the PET beverage bottle industry, although it is more likely to be creep under tension.

Melinex/Mylar are also used in sails. There might also be some data there.

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor