I am looking at using polycarbonate (Bayer Makralon 2458) resin compounded to add colorant for some parts. Unfortunately I don't know the specifics about the colorant/additives. We traditionally EtO sterilize, but are now exploring radiation for speed. Any ideas on if I should expect discoloration issues even though colorant is added? Bayer's brochure suggests that discoloration is only an issue for transparent, colorless parts made from grades that are not stabilized for radiation. I also realize this may be a case by case basis since not all radiation cycles are the same and not all compounded polycarbonate material are created equal. Right now I'm fishing for practical advise.
Any other concerns I should have (or keep in mind) other than discoloration? Are color additives known to change in appearance after being exposed to radiation?
Any other concerns I should have (or keep in mind) other than discoloration? Are color additives known to change in appearance after being exposed to radiation?