Hi to everyone,

I am interested in making a composite mechanical gear for a water pump, comprising of two parts. The first one will be a polymer and the second one rubber which will be vulcanized (in the presence of S) on top of it at 160 degrees Celsius. I have the following questions about the selection of the polymer:

1) Is MINLON (mineral reinforced Nylon 6) a proper selection for the polymer in terms of mechanical characteristics? If not, any other suggestions?

2) The adhesion between MINLON and the rubber part is a crucial characteristic in our application. Will this composite system (polymer-rubber) be able to handle torsional stresses?

3) During the vulcanization process at 160 degrees Celsius, will the MINLON part remain stable?

Thanks in advance
 
Replies continue below

Recommended for you

Eparissis, you ought to know that rubbers are polymers too. I would talk to the manufacturer's technical people about Minlon's stability and other characteristics.
 
I know rubbers are polymers. I am just referring to MINLON as THE polymer because i am interested in MINLON's characteristics specifically. I am in touch with manufacturer's technical people anyway. Thanks for the reply!
 