Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Composite Floor Construction

Status
Not open for further replies.

sengr7

Structural
Nov 15, 2002
2
What or where are the guidelines/recommendations for locating construction joints in a steel and concrete composite slab and beam system?
 
Replies continue below

Recommended for you

Try P300 by the SCI. / MCRMA Technical paper no. 13. (Same book, different publishers)

Page 80 of the above suggest's "Typical pour sizes are up to 1000m2 / day, although there is no technical limitation to the area that may be concreted. Where the limits of the pour do not conicide with permanent slab edges, construction (day joints) are used to define the extent of the pour."

It goes on to suggest that day joints should be over a support position and a butt joint. If this is not possible then no more than 1/3 of a deck span should be left un poured.

A copy of our, Ward Building Components, Multideck Handbook can be downloaded from our web site at and this states/shows the same information with other 'typical' details.

Hope that this helps

Steve
 