Hi
I have been trying to use crippling charts for sizing composite frames before any test data become available, first come to mind was Fig 5.7.2.4 in Mil-HDBK-17F. I later found out by plotting against other data in Mil-17 that the curve in Fig 5.7.2.4 is rather unconservative.
Is there any good literature out there published crippling data for composites. Also, what would be a good paper on crippling test setups.
Thanks
Lenosrep
I have been trying to use crippling charts for sizing composite frames before any test data become available, first come to mind was Fig 5.7.2.4 in Mil-HDBK-17F. I later found out by plotting against other data in Mil-17 that the curve in Fig 5.7.2.4 is rather unconservative.
Is there any good literature out there published crippling data for composites. Also, what would be a good paper on crippling test setups.
Thanks
Lenosrep