May 20, 2020 #1 alurgibon Aerospace Joined Oct 3, 2019 Messages 2 Location BY Give information on the vitality, fatigue of carbon fibers under cyclic loads. How it calculate, testing and design?
Give information on the vitality, fatigue of carbon fibers under cyclic loads. How it calculate, testing and design?
May 20, 2020 #2 SWComposites Aerospace Joined Nov 6, 2000 Messages 3,716 Location US Fatigue is very good. Testing done per ASTM test methods. Upvote 0 Downvote
May 21, 2020 Thread starter #3 alurgibon Aerospace Joined Oct 3, 2019 Messages 2 Location BY Wich test recomandate for this? Upvote 0 Downvote
May 21, 2020 #4 SWComposites Aerospace Joined Nov 6, 2000 Messages 3,716 Location US Please see ASTM D4762, and CMH-17 rev G volume 1. Upvote 0 Downvote