Nov 30, 2004 #1 dpser Chemical Joined Nov 30, 2004 Messages 1 Location IE I was wondering if one would get corrosion problems if 316L stainless steel is used in a purified water generation package that processes brine solution (salty water) Thanks
I was wondering if one would get corrosion problems if 316L stainless steel is used in a purified water generation package that processes brine solution (salty water) Thanks
Dec 2, 2004 1 #2 cub3bead Chemical Joined May 28, 2003 Messages 292 Location US The 300 series stainless steels will usually pit if exposed to elevated Cl levels. This is especially true if the line is left packed with the brine. Upvote 0 Downvote
The 300 series stainless steels will usually pit if exposed to elevated Cl levels. This is especially true if the line is left packed with the brine.