Feb 17, 2004 #1 titogear Mechanical Joined Feb 17, 2004 Messages 1 Location AR I need to know the substantial differences between the ASTM A 106 Gr B Vs.the API 5L Gr.B, above 6" diameter. Thanks a lot.
I need to know the substantial differences between the ASTM A 106 Gr B Vs.the API 5L Gr.B, above 6" diameter. Thanks a lot.
Feb 17, 2004 #2 stanweld Materials Joined May 9, 2003 Messages 2,906 Location US A-106 B is seamless and deoxidized with Silicon. 5L-B may be seamless or welded, deoxidized or not. While A-106 will meet API 5LB, the converse is not. Upvote 0 Downvote
A-106 B is seamless and deoxidized with Silicon. 5L-B may be seamless or welded, deoxidized or not. While A-106 will meet API 5LB, the converse is not.
Feb 18, 2004 #3 PVRV Mechanical Joined Jan 16, 2003 Messages 171 Location KW A106 Gr. B is suitable for high temperature service. Cheers, Upvote 0 Downvote