BigH...if you have to justify your lower compaction, you can point out that "overcompacting" the surface course can lead to "bleeding", which reduces skid resistance and causes premature failure. It's ok to let the traffic do some of your compaction for you over the years, as long as it isn't too much that would lead to rutting.