At constant exposure to high temperatures (e.g. 180 C), many grades of PPS discolor badly. Does anobody know of PPS grades that have superior color stability?
 
Many times discoloration of a polymer is due to the antioxidants and other additives and not the polymer itself.

Can you try masking the color change e.g. using carbon black or TiO2 as pigments?

Chris DeArmitt PhD FRSC CChem

Consultant to the plastics industry
 