Hi everyone,

I have cold bend tubes of SA 213 GR T11 (PARENT METAL NO. 4). Tube size: 50.8mm OD x 4.5mm thik., And bending radius 100.


So, as per IBR code which heat treament cycle shall be follow for stress relieving.
 
What does the IBR Code require? Do you have a copy??
 
Dear mprjapti,

Follow as per B 31.3

Regards.