Jun 2, 2018 #1 mprjapti Materials Joined Jun 2, 2018 Messages 1 Location IN Hi everyone, I have cold bend tubes of SA 213 GR T11 (PARENT METAL NO. 4). Tube size: 50.8mm OD x 4.5mm thik., And bending radius 100. So, as per IBR code which heat treament cycle shall be follow for stress relieving.
Hi everyone, I have cold bend tubes of SA 213 GR T11 (PARENT METAL NO. 4). Tube size: 50.8mm OD x 4.5mm thik., And bending radius 100. So, as per IBR code which heat treament cycle shall be follow for stress relieving.
Jun 2, 2018 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US What does the IBR Code require? Do you have a copy?? Upvote 0 Downvote
Jun 4, 2018 #3 Dhurjati Sen Materials Joined Dec 14, 2017 Messages 1,006 Location IN Dear mprjapti, Follow as per B 31.3 Regards. DHURJATI SEN Upvote 0 Downvote