May 6, 2002 #1 givonz Mechanical Joined Nov 22, 2001 Messages 3 Location HK If possible, could someone tell me the CLTE generally used for Zinc Alloy at 20 degrees. In China and a running a little short on english resources. Cheers givonz
If possible, could someone tell me the CLTE generally used for Zinc Alloy at 20 degrees. In China and a running a little short on english resources. Cheers givonz
May 6, 2002 #2 MortenA Chemical Joined Aug 20, 2001 Messages 2,998 Location DK According to http://www.matweb.com zinc alloys (general) have a CTE of 30 micro m/deg C (20-100 deg C range) Best Regards Morten Upvote 0 Downvote
According to http://www.matweb.com zinc alloys (general) have a CTE of 30 micro m/deg C (20-100 deg C range) Best Regards Morten
May 6, 2002 #3 quark Mechanical Joined Jan 23, 2002 Messages 3,409 Location IN Givonz! It is 26.3X10^-6/deg. C. Note: There is one very good search engine called http://www.yahoo.com . I tried out this link there. http://class.phys.psu.edu/sp02/p213sp02notes/labs/Lab5/Lab5.htm Regards, Upvote 0 Downvote
Givonz! It is 26.3X10^-6/deg. C. Note: There is one very good search engine called http://www.yahoo.com . I tried out this link there. http://class.phys.psu.edu/sp02/p213sp02notes/labs/Lab5/Lab5.htm Regards,
May 6, 2002 Thread starter #4 givonz Mechanical Joined Nov 22, 2001 Messages 3 Location HK Thanks for that people. Cheers Givonz Upvote 0 Downvote