solidman25
Mechanical
- Dec 20, 2010
- 6
I am developing a worm gear assembly that uses a stainless steel worm and a bronze worm gear in combination. The closest thing I can find in my books or online is steel and bronze which only lists a lubricated value of 0.16.
1. Would you suggest using the steel and bronze value
2. Do you have a good source for a coefficient of friction values that do list a stainless steel and bronze coefficient of friction.
2. Do you know why there is no dry/ clean coefficient of friction value listed for bronze and steel?
1. Would you suggest using the steel and bronze value
2. Do you have a good source for a coefficient of friction values that do list a stainless steel and bronze coefficient of friction.
2. Do you know why there is no dry/ clean coefficient of friction value listed for bronze and steel?