Hi Everybody,

According to Code Case 2235-9, (C) state that "The qualification block(s)shall be prepared by welding or HIP......,oriented to simulate flaws parallel to the production weld's fusion line... "

Question 1).The qualification block(s) shall be contain with a welded joint?

Question 2). If the qualification block(s) contain a welded, done welded joint configuration shall be same with production vessel...?

Million thank
 
Replies continue below

Recommended for you

This has been answered already. Please search in this forum.
 
Metengr,
Thanks for you reply. Do you have a guide (with detail)how to make flaws in welded?
 
2468jjcr;
The flaws can be introduced by using EDM notches and flat bottom holes.
 