Our base material Monel400 and weld overlay CoCr-A/Stellite 6 powder, PTA/PAW(Plasma Arc Welding) process.
Pre-heat to 250°C before welding. After welding found to be more porosity & improper fusion.
Please advise for correct procedure.
 
Replies continue below

Recommended for you

Either change your PTA parameters or consider putting down a NiCr (low C) bond layer.

= = = = = = = = = = = = = = = = = = = =