Has anybody ever used Cobra Solid Lubricants for bearings by UTA ?
Wanted to get some feedback...the rep was in here and she made them sound perfect for an application we are looking at, but I tend to take everything with 'a grain of salt' that I hear from reps !!

Any comments would be greatly appreciated...I just hope no UTA reps visit this site to covertly inject good comments into this thread about their product !! LOL !

Thanks !
 
Replies continue below

Recommended for you

I have been using this for about 6 months with standard roller bearings that are get washed thru with a solvent during a process. This of course removed the grease and caused the bearings to sieze. I have not had any problems since changing to Cobra.
 
Status