I am trying to coat a thin layer of lead onto aluminum, to protect the aluminum from battery acid. Any suggestion on how.
 
'Tin' the aluminum with 90-10 (lead-tin) solder. Need a good flux, one specifically for aluminum.
Or, electroplate lead onto tin-plated aluminum.
 