Dec 12, 2006 #1 testingpump Mechanical Joined Dec 12, 2006 Messages 14 Location IL what is the best recommended coating for steel pipes and steel fittings to protect them from water of high salinity.
what is the best recommended coating for steel pipes and steel fittings to protect them from water of high salinity.
Dec 28, 2006 #2 unclesyd Materials Joined Aug 21, 2002 Messages 9,819 Location US With no other information available your best bet would be to checkout Coal Tar Epoxies. I would contact someone like PPG (Coal Cat) with more specifics on your expected environment and see what the have to say. http://www.ppg.com/pafpainttools/PDFS/pghpaints/TDB/97-640.pdf Upvote 0 Downvote