Experts,

What is the limit CO2 partial pressure from where we should take account of corrosion in wet gas pipeline?

Regards,
 
Can you please make your question more elaborate please?
 
On the assumption that the question relates to the minimum threshold, the answer would be: the minimum required by the corrosion model being employed to assess the predicted corrosion rate.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
Thank you, that's what I was looking for.
I am sorry for the bad formulation of the question.
 