We have received a qoutation of CO2 compressor with two options for casing
A- Cast A216ACB with SS lining
B- Forged Steel
I have two questions
1- what should we chose if the two options are with same price and why?
2- regarding the first option, what is the suitable ss lining thickness. We have received different opinion, some say 1.5 mm and some say it can be 4 mm. what is the best practical ss lining thickness
Regards
SHARQ
A- Cast A216ACB with SS lining
B- Forged Steel
I have two questions
1- what should we chose if the two options are with same price and why?
2- regarding the first option, what is the suitable ss lining thickness. We have received different opinion, some say 1.5 mm and some say it can be 4 mm. what is the best practical ss lining thickness