When i cut the ACME thread on CNC Lathe,i face a problem:
the first tooth is a little wider than the others (about 7 teeth totally), as i know that when we use the CNC lathe to cut the thread, there will be a short incorrect threaded length at the beginning and the end,the lengh is depends on machine time constant T,but after i have set the constant to 0.033s, the error still exists,are there any tips for this issue?
Thanks
the first tooth is a little wider than the others (about 7 teeth totally), as i know that when we use the CNC lathe to cut the thread, there will be a short incorrect threaded length at the beginning and the end,the lengh is depends on machine time constant T,but after i have set the constant to 0.033s, the error still exists,are there any tips for this issue?