boffintech
Civil/Environmental
Have a CMU 8" block wall going up.
You can see from the picture that the 15' wide opening has 1 precast lintel beam 8" deep. The plan calls for a 48" deep lintel beam with 3 sets of 2#5 horizontal rebars placed bot/mid/top of the beam.
48" of lintel beam was grouted and with all of rebar; however, the middle and top rebar and grout is discontinuous at the control joints (see picture).
Is this condition an issue?
You can see from the picture that the 15' wide opening has 1 precast lintel beam 8" deep. The plan calls for a 48" deep lintel beam with 3 sets of 2#5 horizontal rebars placed bot/mid/top of the beam.
48" of lintel beam was grouted and with all of rebar; however, the middle and top rebar and grout is discontinuous at the control joints (see picture).
Is this condition an issue?