I am creating sheet metal doors. I am flange bending the four sides then entending the walls up and out.
Is there a way to completly close the corners. Everything I try leaves a small hole at the corners.
I am using Pro/E Wildfire 2.0

John K.
 
Replies continue below

Recommended for you

You have to have "relief" in the corners otherwise the sides would interfere with the adjacent side. You can make the radii of the corners as small as possible to minimize this hole, but there will be a limit to how small you can make it.

Erik
 
WF3 has an automatic corner relief tool as part of the bend dashboard.


"Wildfires are dangerous, hard to control, and economically catastrophic."

Ben Loosli
Sr IS Technologist
L-3 Communications
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor