which type of cleaner (chamical &phisical property) that can i use for cleaning, stopping the rusted area before ipainting with epoxy???
 
What is the initial condition of the steel?
 
Both are used widely. What are the dimensions? Access to abrasive blasting equipment or a tank to immerse in acid?
 
Also What are this steel used for ?
Typical Environments Im 2 / C5-M / C4 ?
Is it carbon steel ? Stainless Steel ... ?
What is the geometry of the steel ? ( Plate / Pipe ...)
 
the type of plate - pressure vessel - carbon steel A516 , or A573 , contain Lpg liquid < thr rusted area external becouse of wet weather
 