Does anyone have any recomendations or procedure for cleaning out the injection screw and barrel for a material change?

There has to be a better way....

Thanks for your time

Aaron
 
The method I use is:

Run extruder until empty.
Purge injection pot.
Fill extruder with new compound and cycle compound into injection pot.
Purge pot.
Repeat.
Purge pot.
Run one cycle on automatic. Check for odd looking defects. If none, continue with production.
 
Purging with the new material usually works although it can be difficult when going from a hard to a soft compound. The problem is knowing for sure the unit is clean; it depend s on how critical it is. I have used uncured natural rubber cleanouts and EPDM cleanouts for critical jobs. No matter what you have to take the time to look around for hung up rubber. Sometimes pulling everything apart is necessary.
 
normally, the use of virgin resin (same with compound but no additive) is rent to pruge
 