MikeKostiz
Civil/Environmental
I am looking for information on sewer clay pipe failure. I am working on a sewer rehabilitation project that will involve removing and replacing 50-60 year old clay pipe that has been described as having longitudinal and circumferential cracking. I suspect that the cracking is caused by tree roots. I am looking for testing that has been done to determine what kind of pressure tree roots can exert to crack and displace 6"-8" clay pipe and cause the cracking noted above. I would be also interested in the type of cracking that results from soil and traffic loading. Thanks!