We are currently buying spacers according to ASME Code Sect.II-A SA 193 Gr B8T material.
Specification SA 193 does not mention spacers but bars, wires, fasteners, bolts,...
Our spacers can be described as bars with reduced diameter on both ends (for about 20mm).
Are these spacers classified as bars?
 