I have an E-beam weld joint between a bellows and a ring with the configuration shown in the attachment. I have an acceptance criteria of underfill shall be less than 10% of the joint thickness (ref. AMS 2681 para 3.7.6). Is the joint thickness defined by the depth of penetration specified (20mils) or joint thickness as shown in Figure 1? The vendor left a significant crater as shown in Figure 2. That crater is well below the original joint line. Is the threshold 2 mils (10% of 20mils) or 1.6 mils (10% of 16 mils)?