It is broadly recommended that you do not attempt to bond bearing pads in place.
The technique can be difficult due to the use of anti ozonants in the rubberr compound, and if the ' adhesive ' fails, the co-efficient of friction reduces and thus the bearing can more easily slip out.
If you restrain by confining part of the rubber thickness, then the permitted shear deformation is reduced.
An exact answer would be governed by the overall thickness of the ' bearing ' pad you nominate.
So far as the other answer is concerned, a POT BEARING requires totally different ' restraiint ' compared to a bearing pad.