Material: Carbon Steel + Inconel 625 Clad
pipe 12" schedule 160 [323.85 OD x 33.32mm thk](Cladded -Weld overlayed inside all over),fittings and flanges are to be girth welded at site.
Internal Clad weld is Er NiCr mo 3 3mm thick.
Now i have to weld the Girth seams.
Code is ANSI/ASME B 31.3.
After welding the Girth seam fully with Er Ni Cr mo3 + E NiCr Mo 3 is it necessary to perform PWHT?
Reason for the question:
1)The table in 31.3 gives P number and F Number and PWHT temp and Soaking Time.
2)After Corrosion resistant overlay one does not require PWHT so long as corrosion resistant overlay is done with pre heat.If i choose to overlay the edges by pre heating then i make the edge (that is Buttering) and then weld the Butt joints, do i still need PWHT? (subjecting all procedures qualified one to one)
pipe 12" schedule 160 [323.85 OD x 33.32mm thk](Cladded -Weld overlayed inside all over),fittings and flanges are to be girth welded at site.
Internal Clad weld is Er NiCr mo 3 3mm thick.
Now i have to weld the Girth seams.
Code is ANSI/ASME B 31.3.
After welding the Girth seam fully with Er Ni Cr mo3 + E NiCr Mo 3 is it necessary to perform PWHT?
Reason for the question:
1)The table in 31.3 gives P number and F Number and PWHT temp and Soaking Time.
2)After Corrosion resistant overlay one does not require PWHT so long as corrosion resistant overlay is done with pre heat.If i choose to overlay the edges by pre heating then i make the edge (that is Buttering) and then weld the Butt joints, do i still need PWHT? (subjecting all procedures qualified one to one)