Hi friends
Well here is the case -
After cladding of pipe and flange with all approved WPS we carried out NDT ( UT for dis- bonding and PT for open surface defects as per approved procedure with approved NDT technicians ) and same was witnessed , accepted and released by vendor inspector as well as client inspector also for spooling activity.
After butt welding ( Flange to Pipe ) we took RT for butt weld and we found some linear line ( having width more nearly 2~3 mm ) and porosity ( dia nearly 6 ~ 7 mm ) in clad area. Kindly note that butt weld area is free from any defects/ indication.
Questions are -
1- Is this clad defects treated as butt weld defects ( acceptance and rejection )
2- If this clad defects are rejected then what about those cladded area where there is NO RT ?
3- what would be rejection / acceptance criteria for clad defects in radiography ? ( kindly refer if any code is there for RT in cladding )
further more information on this issue is hearty welcomed.
Thanks
Well here is the case -
After cladding of pipe and flange with all approved WPS we carried out NDT ( UT for dis- bonding and PT for open surface defects as per approved procedure with approved NDT technicians ) and same was witnessed , accepted and released by vendor inspector as well as client inspector also for spooling activity.
After butt welding ( Flange to Pipe ) we took RT for butt weld and we found some linear line ( having width more nearly 2~3 mm ) and porosity ( dia nearly 6 ~ 7 mm ) in clad area. Kindly note that butt weld area is free from any defects/ indication.
Questions are -
1- Is this clad defects treated as butt weld defects ( acceptance and rejection )
2- If this clad defects are rejected then what about those cladded area where there is NO RT ?
3- what would be rejection / acceptance criteria for clad defects in radiography ? ( kindly refer if any code is there for RT in cladding )
further more information on this issue is hearty welcomed.