phil23,
If you can prove that the 150# flange was not permanently damaged during the hydrotest, will you use it for Class 600# pipe rating, with the wrong flange hanging on the end of the pipe spool?
If not, what's the point of identifying the degree of damage on a useless flange, when you'll have to replace it regardless of damage or not.
However, if you intend to salvage the flange for second hand application, think twice. It might prove dangerous.