I have a fabrication that requires CJP welds for moment connections in a grillage type frame. (Basically welding two wide flange shapes perpendicular to each other.) The intended use of the fabrication is underwater and we typically call to seal weld all joints to minimize corrosion. The CJP weld on the top flange is designed as a single bevel with backing bar. Can we fillet weld the backing bar in place to minimize corrosion or is this going to place a stress concentration at the backing bar? My other option is to remove the backing bar which will add considerable work to the job. Final option is to qualify welders with ceramic backing bar