Does the exposure of Vinyl Ester Resin to environment safe? no harmful effect? i am planning of using this as a resin for my fiber reinforced plastic. thanks.
 
Replies continue below

Recommended for you

What's your question? Is it safe for the vinyl ester or the environment? What's the environment? Is it 15% sulfuric acid? Are you planning on eating it?
By the way, this is a civil engineering forum, not the poorly formatted question forum.
 
Well, the forum is actually the civil/environmental forum, but the question needs clarification.
Will you be discharging the resin via air or water waste? Will solid waste be generated?
What does the MSDS say about exposure levels for the workers who will be handling the material?
What kinds of quantities are you anticipating using? Is this a one time deal or an ongoing process?
 
suppose you should develop a SWP for its use and consult with your local regulatory agencies to make sure you comply
This material is considered hazardous by the OSHA Hazard
Communication Standard (29 CFR 1910.1200)
WARNING!
CONTAINS STYRENE
POSSIBLE CANCER HAZARD - MAY CAUSE CANCER BASED ON ANIMAL DATA
HARMFUL IF INHALED, ABSORBED THROUGH SKIN, OR SWALLOWED
CAUSES SKIN AND EYE IRRITATION
FLAMMABLE LIQUID AND VAPOR
MAY FORM EXPLOSIVE PEROXIDES
MAY POLYMERIZE
Personal Precautionary Measures: Avoid breathing vapor. Avoid contact with eyes, skin, and clothing.
Do not taste or swallow. Use only with adequate ventilation. Wash thoroughly after handling.
 