circular finish requirement

Status
Not open for further replies.

johnmoore

Mechanical
Jul 26, 2007
1
Can someone define "circular finish" I have a customer drawing requiring a 16 finish or 32c.

thanks
 
Replies continue below

Recommended for you

how do you check a 32 circular finish
across the grain or with direction of circular finish
how would you check the depth of variation and how much
depth could you have,i figured .00032 depth
 
You check across the grain, or in the direction which will give the maximum deviation (surface finish requirements are default "max" allowable, unless two are specified (upper and lower limits).

A 32 is 32 micro-inches rms. You sweep a (usually) electronically-amplified stylus across a 1-inch swath of the surface, and take an rms (root-mean-square) average of the reading. Alternatively, purchase a visual comparison standard.
 