Easy one for somebody I reckon:

I have a chs which cantilevers out from a flat plate. It is fully welded to the plate with a fillet weld around its perimeter. How do I calculate the moment capacity of this connection? I have done 'what I think' is right, but it has now become the critical location which limits the load capacity so I need to check my method. I have a fixed weld size and the known weld transverse capacity.
 
Replies continue below

Recommended for you

In "Design of Weldments" by Blodgett, he has an example for a fillet weld about a round section to a flat plate. See 6.3-14 in the book. It takes a small amount of modification because the example has stiffeners, but you should get the gist of it.