Greetings, I have Chrysler Process Standard for welding nuts but not for welding bolts.

I have 2 stampings (1.5mm thick) that I am welding a M6x1 weld bolt in. Need guidance on push-off capabilities.

Thanks,

richards49323
 
Chrysler Process Standard PS-1791 WELD SCREWS - PROJECTION WELDING. For M6 in 1.5 mm thick steel, the minimum strength requirement is 10230 N.
 
Good Morning, Would you by any chance of a copy of this, Chrysler Process Standard PS-1791 WELD SCREWS - PROJECTION WELDING.

I cant seem to locate it.

Thanks again,

richards49323
 