Hi there,
I am looking for a source of metal material recommendations for a tank to be filled with Chromic and Arsenic acid with water. A pointer in the right direction would be appreciated.
Thanks
 
Replies continue below

Recommended for you

What temperature and what concentrations for the acids?
 
Thanks for the reply. The temperature is 40°C max and 33% of each acid and then 33% water.
 