I have to make some rolled rings (70 mm thick) 2.5 m diameter. The only thing that i know about the material is 13CrV4. I can't find it. Can anyone give me any info. I need the mechanical proprieties to see what would be the force needed and if there are any risks for cracking. I need this tonight :)

Thanks for your help.

Calin
 
Are you sure with the material designation? 13CrV4? Perhaps 13CrMoV4?
 
Sorted out. I checked with the customer. It is 13CrMoV4. Thanks.

I feel stupid now. It was my first post. But it helped.
 