All,

I am looking for the pros and cons comparing 52CrMoV4 1.7701, 5160, and 6150 for spring application.

Currently have a requirement for 5,000 minimum cycle life, with stress levels at 136,000 lbs/in^2 at the top of its working deflection (bar dia of 2.687"). Possible saline conditions. Temperatures from 34F-151F.

Thanks in advance,

mgh
 
Replies continue below

Recommended for you

So in terms of crack growth, fatigue, and modulus all three are pretty similar. No real difference then?
 
Don't think so. 6150 has got more tensile strength than 5160. Others may confirm please.
 