Hello all, I have two analysis of two samples of parts of a farming machinery and I want you to help me to find what type of steel are. Here you will find the results of the chemistry.
SAMPLE ONE: 0.366 C; 0.77 Mn; 0.256 Si; 0.011 P; 0.036 S; 0.81 Cr; 0.085 Ni; 0.014 Mo; 0.262 Cu; 0.004 Al
SAMPLE TWO: 0.337 C; 0.69 Mn; 0.205 Si; 0.010 P; 0.018 S; 0.11 Cr; 0.115 Ni; 0.017 Mo; 0.211 Cu; 0.0024 Al
I hope you can help.
Thanks in advance
Best regards
Daniel Nava
SAMPLE ONE: 0.366 C; 0.77 Mn; 0.256 Si; 0.011 P; 0.036 S; 0.81 Cr; 0.085 Ni; 0.014 Mo; 0.262 Cu; 0.004 Al
SAMPLE TWO: 0.337 C; 0.69 Mn; 0.205 Si; 0.010 P; 0.018 S; 0.11 Cr; 0.115 Ni; 0.017 Mo; 0.211 Cu; 0.0024 Al
I hope you can help.
Thanks in advance
Best regards
Daniel Nava