I just recently started working in a steel Foundry, I'm not familiar with the Charpy Test. I have read some specs(asme sa352 for grade LCC and A-370. Recently we've seen failures in one of the tree test bars. The bars are being poured in a sandcasting mold. Would you know what could make them fail?
Thanks for the help! Mario