I have SA-516-70N plate that says on the MTR it was charpy impact tested at -30F.
MDMT is -40 F.
Based on my design calculations, charpy impact testing is not required for my MDMT of -40F.
In my opinion, there should be no problem using this plate for -40 F but I'm being told that since the MTR says it was tested at -30 F, the plate is not good for -40 F. This doesn't make sense since the plate would be good for -40 F if it had no charpy test shown on the MTR.
Am I wrong?
MDMT is -40 F.
Based on my design calculations, charpy impact testing is not required for my MDMT of -40F.
In my opinion, there should be no problem using this plate for -40 F but I'm being told that since the MTR says it was tested at -30 F, the plate is not good for -40 F. This doesn't make sense since the plate would be good for -40 F if it had no charpy test shown on the MTR.